Grades und Performance

drawing-die-1drawing-die-2drawing-die-3

Klasse

Dichte(g/cm3)

Härte(HRA)

Biegefestigkeit(Mpa)

Koerzitivkraft (KA/m)

YL01

15.15~15.30

≥1930

≥1900

30.0~38.0

YL05.1

14.86~15.05

≥1770

≥2200

27.0~33.0

YL 10.2

14.40~14.55

1550~1650

≥2000

18.4~22.5

YG6X

14.85~15.05

≥91.0

≥1560

19.0~26.0

YRL10

14.90~15.04

≥1500

≥2500

13.5~18.0

YG3

15.20~15.40

≥90.5

≥1300

16.0~19.5

YG6

14.85~15.05

≥89.5

≥1670

11.0~16.0

YG8

14.65~14.85

≥89.0

≥1840

10.0~15.5

YG11

14.30~14.50

≥87.0

≥2200

7.0~14.0

YG15

13.95~14.15

≥86.5

≥2400

7.0~11.0

MA30

14.85~15.05

≥89.7

≥2000

11.0~16.0

MA30A

14.65~14.85

≥89.2

≥2300

10.0~15.5

MA10

14.77~14.87

2050~2200

≥3300(C式样)

36.0~38.0